Brand:

Ador Automig MC 70C-6M E70C-6M Metal-Cored Wire

Description

Metal-cored wire for automated carbon steel welding with Ar-CO2

The Ador Automig MC 70C-6M is a metal-cored wire classified AWS A5.18 E70C-6M H4 and EN ISO 17632-A T 46 4 M M21 3 H5. Ador lists good weldability with minimal or no slag, excellent bead appearance, a high deposition rate, suitability for single and multi-pass welding, exceptional mechanical properties at low temperatures, and a best fit for automated and robotised applications.

Technical specifications

Parameter Specification
Manufacturer / product Ador Welding / Automig MC 70C-6M
Process MCAW C-Mn steel, gas-shielded
AWS classification A5.18 E70C-6M H4
EN ISO classification 17632-A T 46 4 M M21 3 H5
Approvals listed CE
Undiluted weld metal, typical % C 0.06, Mn 1.45, Si 0.4
Tensile strength, as welded (typical) 585 MPa
Yield strength at 0.2% offset 490 MPa
Elongation 28%
Charpy V impact at -40 °C 60 J
Diffusible hydrogen Under 4 ml/100 g
Diameters 1.2 and 1.6 mm
Net weight 15 kg
Polarity / positions DCEP; flat butt and fillet welds only
Shielding gas 80Ar+20CO2 at 15-20 l/min

Typical applications

The data sheet lists welding of carbon and C-Mn steels including fine-grained steels, shipbuilding, boilers, pressure vessels and pipe steels. It also names suitability for joining SA 36/36M (P No. 1) and SA 285/285M Grades A, B and C (P No. 1).

How a metal-cored wire differs from a rutile cored wire

The core is mostly metal powder with little slag former, so the bead is nearly slag-free and multi-pass welds can be laid without chipping between passes. Deposition efficiency is higher than a solid wire because the arc spreads over a wider area of the tubular sheath, giving a broader penetration profile and good sidewall fusion. The compromise is positional limitation: Ador lists flat butt and fillet welds only, so the wire is not intended for vertical or overhead use.

With a low diffusible hydrogen figure under 4 ml per 100 g, the wire helps limit cold-cracking risk on thicker sections, though preheat rules from your procedure still apply. Keep a steady contact-tip-to-work distance and set voltage to hold spray transfer in the 80/20 argon-CO2 mixture. On mechanised carriages, constant travel speed makes the most of the nearly slag-free bead.

For a solid wire in the same C-Mn class, see KISWEL KC-28 ER70S-6; this metal-cored grade is the one to consider when deposition rate and automation are priorities.

How the Automig MC 70C-6M metal-cored wire works

The Automig MC 70C-6M is a tubular wire whose core holds mainly iron powder and alloying elements rather than slag formers. In the arc, the core and sheath melt together to give the C-Mn deposit shown in the table above, while the 80% argon / 20% CO2 gas shields the pool. Only small silicon islands form on the bead surface, so multi-pass welds can be laid with little or no interpass cleaning. Ador lists good weldability with minimal or no slag, excellent bead appearance and high deposition, and names automated and robotised welding as the best fit.

Base metals and industries named by Ador

  • Carbon and C-Mn steels, including fine-grained steels.
  • Shipbuilding, boilers, pressure vessels and pipe steels.
  • SA 36/36M and SA 285/285M Grades A, B and C (P No. 1).

Selecting and ordering the E70C-6M wire

Item Ador data
Diameters 1.2 and 1.6 mm
Net weight 15 kg
Polarity DCEP
Shielding gas 80Ar+20CO2, 15–20 l/min
Positions Flat butt and fillet welds only
Impact 60 J at −40 °C (typical)

The 60 J typical Charpy result at −40 °C and the H4 hydrogen designation make the wire a candidate for pressure parts and structures that need low-temperature toughness. As with any typical value, confirm the batch test certificate if the specification sets a minimum.

Setting up for mechanised welding

  • Use smooth or knurled rolls suited to tubular wire with moderate pressure.
  • Fix the torch angle and contact-tip-to-work distance on the carriage or robot.
  • Check gas flow at the nozzle, not only at the regulator.
  • Brush off the small silicon deposits before the final pass if a paint system follows.
  • Keep the wire in its packaging until it is loaded on the feeder.

Metal-cored wire for fabrication in Oman and the GCC

Boiler, vessel, pipe spool and shipyard fabricators in Oman and the GCC adopt metal-cored wire to raise productivity on mechanised lines. Seven Star LLC supplies the Ador Automig MC 70C-6M across Oman and the GCC. Our team can help confirm the correct ordering code for the diameter you need.

Reading the E70C-6M H4 and T 46 4 M M21 3 H5 classifications

In AWS A5.18, the E means an electrode, the 70 a minimum tensile strength of 70 ksi, the C a composite (metal-cored) wire, the 6 the chemistry and impact group, the M a mixed argon-CO2 gas, and H4 a diffusible hydrogen level below 4 ml per 100 g. The EN ISO 17632-A designation T 46 4 M M21 3 H5 reads as a tubular wire with 460 MPa minimum yield, 47 J at −40 °C, a metal-cored type, mixed gas M21, use in flat butt and fillet welds (position 3) and hydrogen below 5 ml per 100 g. Together they explain why the data sheet limits the wire to flat butt and fillet positions while giving good toughness at low temperature.

When the procedure is qualified with this wire, record the gas mixture, flow, wire diameter and current range used, so that production welds can repeat the same conditions and the mechanical properties shown on the test coupon.

Documents and quotation

The official Ador Automig MC 70C-6M data sheet is available from the link below. Related consumables are listed in our Flux-Cored Welding Wire category.

To request a quote, send the diameter or size, pack type, quantity and any certificate or approval requirement.

Datasheets & Documents
  • PDF Datasheet Ador Automig MC 70C-6M product data sheet Download
Reviews (0)

Reviews

There are no reviews yet.

How would you rate this product?

It takes about 10 seconds — just tap a star. Your email is never published.

About brand

Ador Welding is the Indian manufacturer of welding consumables and welding equipment: covered electrodes, TIG rods, solid, flux-cored and metal-cored wires, submerged arc consumables and welding machines. It was incorporated on 22 October 1951 as Advani-Oerlikon Ltd, a joint venture between J B Advani & Co. and the Swiss Oerlikon-Bührle group, set up to make welding electrodes for India. The name changed to Ador Welding Ltd in October 2003; the company is based in Mumbai, belongs to the Ador Group and is listed in India.

Seven Star LLC sources and supplies Ador welding electrodes, TIG rods and MIG wires for fabricators and contractors in Oman, quoting each item by product name, AWS classification and size.

Ador Welding company profile

Incorporated 22 October 1951, as Advani-Oerlikon Ltd
Founding partners J B Advani & Co. (India) and the Oerlikon-Bührle group (Switzerland)
Renamed Ador Welding Ltd, 16 October 2003
Headquarters Mumbai, India
Ownership Ador Group company, listed on the Indian stock exchanges
Product families Celwel, Supabase and Tenalloy electrodes, Tigfil and Tiginox TIG rods, Automig solid, flux-cored and metal-cored wires, submerged arc wires and fluxes, inverter welding machines

Milestones

  • 1951: Advani-Oerlikon Ltd is incorporated on 22 October to make welding electrodes in India.
  • 2003: The company is renamed Ador Welding Ltd on 16 October.

Ador Welding consumables listed here

The listed Ador electrodes and wires are grouped by the steel they join:

  • Carbon steel, low hydrogen: Supabase X Plus (E7018 H4R) and Tenalloy Z Plus (E7018-1)
  • Cellulosic pipeline electrodes: Celwel 60 (E6010), Celwel 70P (E7010-P1) and Celwel 80P (E8010-P1)
  • Creep-resistant chrome-moly: Cromoten (E8018-B2), Cromoten C (E9018-B3) and Cromoten 9M-15 (E9015-B91) for P91
  • Weathering steel: Ultracorten I (E7018-W1)
  • Duplex and super duplex stainless: Betanox 4462 and Betanox 2594 electrodes, Tiginox 2209 and 2594 TIG rods, Miginox 2209 MIG wire

Where Ador electrodes are used

Cellulosic Celwel grades are used for root and hot passes on cross-country pipelines. Low hydrogen E7018 types serve structural steel, pressure vessels and piping. Cromoten grades are for boiler tubes, headers and steam lines in power and refinery units, and the 2209 and 2594 fillers are for duplex piping in seawater, produced water and process service, which is common in the GCC.

Ador Welding products we list

Family Examples
Welding Electrodes Betanox 2594-16 E2594-16 Super Duplex, Betanox 4462 E2209-16 Duplex Stainless Steel, Cromoten 9M-15 E9015-B91 P91 Welding Electrode, Cromoten C E9018-B3 2.25Cr-1Mo Creep, Cromoten E8018-B2 1.25Cr-0.5Mo Low Alloy, Supabase X Plus E7018 H4R Low Hydrogen, Tenalloy Z Plus E7018-1 H4R Pipe Welding, Ultracorten I E7018-W1 Weathering Steel
TIG Welding Wire Tigfil 70S-6 ER70S-6 Carbon Steel TIG Welding, Tigfil 90S-B3 ER90S-B3 Chrome-Moly TIG, Tiginox 2209 ER2209 Duplex Stainless TIG, Tiginox 2594 ER2594 Super Duplex TIG Welding, Tiginox 316L ER316L Stainless TIG Welding Rod
Flux-Cored Welding Wire Automig FC 71T-1 E71T-1C Rutile Flux-Cored, Automig FC 91T1-B3 Chrome-Moly Flux-Cored, Automig MC 70C-6M E70C-6M Metal-Cored Wire, Miginox FC 316L E316LT1-4 Stainless
Cellulosic Pipeline Electrodes Celwel 60 E6010 Cellulosic Pipeline Welding, Celwel 70P E7010-P1 Cellulosic Pipeline, Celwel 80P E8010-P1 High Strength Pipeline
Solid Welding Wire Automig 90S-B3 ER90S-B3 Chrome-Moly MIG, Miginox 2209 ER2209 Duplex Stainless MIG

Ordering Ador consumables: what we need

Give the Ador product name and the AWS classification together, the diameter and length, the quantity in kilograms or packets, and the packing you require. Vacuum packing matters for low hydrogen and chrome-moly electrodes. State the welding procedure or code that governs the job and any requirement for impact testing, diffusible hydrogen level, ferrite or corrosion testing. If your client needs a batch test certificate of a defined type, say so at the inquiry stage, because it is requested from the manufacturer for the specific batch.

Facts checked against Ador Welding's company filings and published profiles, October 2026.

FAQ

Questions about the Ador Automig MC 70C-6M E70C-6M Metal-Cored Wire

Answers from our engineering team on installation, compatibility and integration.

01What is the AWS classification of Ador Automig MC 70C-6M?
AWS A5.18 E70C-6M H4, with EN ISO 17632-A T 46 4 M M21 3 H5.
02Which shielding gas is used?
80Ar+20CO2 at 15-20 l/min on DCEP.
03Which positions are listed?
Flat butt and fillet welds only.
04What impact value is typical?
60 J at -40 C.
05What diffusible hydrogen level is stated?
Under 4 ml per 100 g.