Böhler Thermanit MTS 3 LNi EB91 P91 Submerged Arc Wire

Description

P91 creep-resistant SAW wire for power generation

Böhler Thermanit MTS 3 LNi is a solid wire for submerged arc welding of creep-resistant P91 steel in power generation, with the data sheet noting a limited Mn plus Ni content below 1 %. It is classified AWS A5.23 / SFA-5.23 EB91 and EN ISO 24598-A S S ZCrMo91. The typical analysis is a modified 9Cr-1Mo composition with vanadium, niobium and nitrogen, so the weld metal matches P91 base material in main steam piping, headers, superheater and reheater components.

Technical specifications

Parameter Specification
Product type SAW wire, low alloyed, creep resistant, solid
AWS classification A5.23 / SFA-5.23 EB91
EN ISO classification 24598-A S S ZCrMo91
Typical wire analysis, wt % C 0.11; Si 0.25; Mn 0.65; Cr 9.0; Mo 0.95; V 0.20; Nb 0.06; N 0.045
Special feature Mn + Ni below 1 %
Application Creep-resistant P91 steel in power generation
Diameters, inch (US data sheet) 3/32; 1/8
Approvals on data sheet None listed

Flux and procedure

For the related Thermanit MTS 3 wire, Böhler’s global data sheet recommends

Marathon 543.

, and Marathon 543 is described as a flux for P91, P92 and similar 9 % Cr steels. For this LNi version the US data sheet itself gives no flux, so confirm the pairing with your WPS. The usual P91 discipline applies: controlled preheat and interpass range, defined cooling before PWHT, tempering at the qualified temperature, and hardness or impact checks required by the code. A restricted Mn plus Ni content raises the temperature at which the weld metal begins to transform on heating, which leaves more margin when the post-weld treatment is performed, a point that depends on the specification of your project.

Related Böhler SAW wire AWS / EN ISO class Typical steel
Union S 2 CrMo EB2R / S S CrMo1 1.25Cr-0.5Mo boiler and vessel steel
Union S 1 CrMo 2 EB3R / S S CrMo2 2.25Cr-1Mo, grade 22 hydrocrackers
Union S 3 NiMo 1 EF3 / S3Ni1Mo Fine-grained steels, Ni-Mo wire

Storage and wire handling

Copper-coated SAW wire protects itself from rust only while it stays dry and clean. Keep spools and coils in their original packing until use, store them off the floor in a dry room, and do not leave an opened spool on the machine overnight in humid conditions. Surface rust and dust shorten contact tip life, disturb feeding and add hydrogen to the weld. Before ordering, confirm the diameter, spool or coil type and the certificate level (for example EN 10204 type 3.1) that your project requires.

How Böhler Thermanit MTS 3 LNi submerged arc wire works

Submerged arc welding feeds a solid wire into a bed of granular flux, and the arc burns under the flux. The flux melts into a slag that protects the weld metal and shapes the bead, and the wire supplies the alloy. This wire has a modified 9Cr-1Mo analysis with vanadium, niobium and nitrogen, which gives creep strength at the temperatures of a power plant steam system. The data sheet notes a limited manganese plus nickel content below 1 %, which relates to the transformation behaviour of the weld metal during post-weld heat treatment.

Where Thermanit MTS 3 LNi is used

  • Main steam piping and headers in power generation.
  • Superheater and reheater components.
  • Fabrication in creep-resistant P91 steel.
  • Thick sections where submerged arc gives high deposition.

Selection checklist for Thermanit MTS 3 LNi

  • Base material: P91 or a matching 9 % chromium creep-resistant steel.
  • Classification: AWS A5.23 / SFA-5.23 EB91 and EN ISO 24598-A S S ZCrMo91.
  • Wire diameter: 3/32 or 1/8 inch on the data sheet.
  • Flux: the US data sheet gives none for this version, so confirm the pairing with the welding procedure.
  • Mn plus Ni limit of 1 %, if the project specification asks for it.
  • Procedure qualification, post-weld heat treatment and testing demanded by the code.
  • Packaging and spool size for the welding head.

Welding, handling and quality notes

P91 welding needs discipline: controlled preheat and interpass temperature, defined cooling before post-weld heat treatment, tempering at the qualified temperature, and hardness or impact checks required by the code. Keep spools dry in their packing, and store flux dry as well. Clean the joint before welding, record parameters, and follow the welding procedure without shortcuts, since errors in P91 welds can show up as early service problems.

Requesting a quotation for the Böhler Thermanit MTS 3 LNi

Send the wire diameter, quantity, spool type and your planned flux. Seven Star LLC serves industrial customers in Oman and the GCC and replies with a quotation based on the information provided.

Flux pairing for P91 welding

For the related Thermanit MTS 3 wire, the global data sheet recommends the Marathon 543 flux, described as a flux for P91, P92 and similar 9 % chromium steels. For this LNi version, the pairing is confirmed through the welding procedure, so ask for the data of the flux you plan to use.

Records and testing for P91 welds

Keep the welding procedure, the welder qualification, the heat treatment chart and the hardness test results with the weld records. For power plant piping, the owner or the inspector often requests this file, so confirm what is required before welding starts.

Wire diameter and welding parameters

The wire is offered in 3/32 and 1/8 inch diameters. A smaller wire suits thinner sections and lower current, while a larger wire raises deposition. Set the current, voltage and travel speed from the qualified procedure, and do not exceed the heat input limits of the specification.

Documents and quotation

The Böhler Welding data sheet for Thermanit MTS 3 LNi (SAW, US edition, 05/2021) is attached. See the SAW Wire category. For a quotation, send diameter, packaging, quantity and the certificate and PMI requirements.

Datasheets & Documents
  • PDF Datasheet Böhler Welding Thermanit MTS 3 LNi SAW wire data sheet (US edition, 05/2021) Download
Reviews (0)

Reviews

There are no reviews yet.

How would you rate this product?

It takes about 10 seconds — just tap a star. Your email is never published.

About brand

Böhler Welding is the welding consumables and equipment brand of voestalpine Böhler Welding, part of the Austrian steel and technology group voestalpine. Its roots go back to 1870, when the brothers Albert and Emil Böhler founded the Böhler company in Vienna; in 1894 they bought the steel works in Kapfenberg, Styria, which became the home of Böhler special steels and, later, Böhler welding filler metals. Welding became a separate division of the newly formed Böhler-Uddeholm group in 1991. voestalpine took over Böhler-Uddeholm in 2007, and the welding business, headquartered in Düsseldorf, Germany, has been part of voestalpine's Metal Engineering Division since 2013.

Böhler Welding company profile

Origins 1870, Vienna, Austria: Albert and Emil Böhler found the Böhler company; Kapfenberg steel works acquired in 1894
Welding business Separate division of Böhler-Uddeholm from 1991 (the same year it acquired UTP)
Ownership voestalpine AG (Linz, Austria), which took over Böhler-Uddeholm in 2007; welding integrated into the Metal Engineering Division in 2013
Headquarters Düsseldorf, Germany (voestalpine Böhler Welding); Austrian company seated in Kapfenberg
Brands in the group Böhler Welding (joining consumables and welding machines), UTP Maintenance (repair and hardfacing), Fontargen Brazing; product lines such as FOX, Thermanit, Union, diamondspark, FOXcore, Marathon and UV fluxes
Product families Stick electrodes, TIG rods, MIG/MAG solid wires, flux-cored and metal-cored wires, submerged arc wires and fluxes, welding machines and plasma cutters

Milestones

  • 1870: Albert and Emil Böhler found the company in Vienna.
  • 1894: The Kapfenberg cast steel works is purchased.
  • 1991: Böhler Welding becomes a separate division of Böhler-Uddeholm and acquires UTP.
  • 2007: voestalpine makes its takeover offer for Böhler-Uddeholm.
  • 2013: The welding business is integrated into voestalpine's Metal Engineering Division as voestalpine Böhler Welding.

Choosing Böhler welding consumables

The filler metal must match the base metal and the service. Carbon steel pipe is often welded with a cellulosic root (FOX CEL+, AWS E6010) because it penetrates well in vertical-down welding, followed by low-hydrogen fill and cap passes (FOX EV 50, E7018-1, or FOX BVD vertical-down electrodes). Creep-resistant chromium-molybdenum steels need matching consumables and controlled preheat and post-weld heat treatment: for example FOX DCMS Kb (E8018-B2) for 1.25Cr-0.5Mo, FOX CM 2 Kb (E9018-B3) for 2.25Cr-1Mo and Thermanit Chromo 9 V Mod for P91. Duplex stainless steel uses an over-alloyed 2209 filler (FOX CN 22/9 N-B, Thermanit 22/09) to keep the ferrite-austenite balance. Low-hydrogen electrodes must be stored dry and re-baked according to the data sheet.

Where Böhler Welding products are used

In Oman and the GCC, Böhler consumables are used on cross-country pipelines, oil and gas facilities, refineries and petrochemical plants, power and desalination plants with P91 and Cr-Mo piping, pressure vessel and tank fabrication, and structural steel work.

Böhler Welding products we list

Family Examples
Stick electrodes FOX CEL+ E6010, FOX EV 50, FOX EV PIPE, FOX BVD 85, FOX DCMS Kb, FOX CM 2 Kb, FOX CN 22/9 N-B, Thermanit Chromo 9 V Mod
TIG rods EMK 6, Union ER 80S-B2, Union ER 90S-B3, Thermanit GE-316L, Thermanit 22/09, Thermanit 309L
Flux-cored and metal-cored wires FOXcore 71 RC, diamondspark 52 RC, diamondspark X70 RC-Pipe, FOXcore 316L-T1, FOXcore 2209-T1
Submerged arc wires and fluxes Union S 2 Si, Union S 3 Si, Union S 1 CrMo 2, Thermanit MTS 3 LNi, UV 418 TT, Marathon 543
Welding and cutting machines TERRA 500 RC, TERRA NX 400 TLH, TERRA NX 500 PME, SABER 70 CHP

Ordering Böhler Welding products: what we need

Send the product name and AWS or EN classification (for example FOX EV 50, AWS A5.1 E7018-1), the diameter and the quantity in kg. For project work, tell us the base material, welding process and any certificate needed, such as an EN 10204 3.1 inspection certificate.

Facts checked against voestalpine's published company histories, October 2026.

FAQ

Questions about the Böhler Thermanit MTS 3 LNi EB91 P91 Submerged Arc

Answers from our engineering team on installation, compatibility and integration.

01What is the classification of Thermanit MTS 3 LNi?
AWS A5.23 EB91 and EN ISO 24598-A S S ZCrMo91.
02Which steel does it weld?
Creep-resistant P91 steel in power generation.
03What does LNi mean on this wire?
The data sheet notes Mn plus Ni below 1 %.
04Which diameters does the US sheet list?
3/32 and 1/8 inch.
05Which flux is recommended?
Marathon 543 for the related Thermanit MTS 3 wire; confirm the pairing for your WPS.